- Table K-1 to Subpart K of Part 98—Electric Arc Furnace (EAF) CH4 Emission Factors
Alloy product produced in EAF | CH (kg CH | EAF Operation | Batch-charging | Sprinkle-charging a | Sprinkle-charging and
>750 °C b | Silicon metal | 1.5 | 1.2 | 0.7 | Ferrosilicon 90% | 1.4 | 1.1 | 0.6 | Ferrosilicon 75% | 1.3 | 1.0 | 0.5 | Ferrosilicon 65% | 1.3 | 1.0 | 0.5 |
---|
a Sprinkle-charging is charging intermittently every minute.
b Temperature measured in off-gas channel downstream of the furnace hood.